Fluffy Foam Shampoo

Formulation Table

Phase Ingredient INCI Purpose %
A Water Balance
Polyquaternium-10 Conditioning; thickener 0.50
B ANON BDF-R Cocamidopropyl Betaine, Water Improves detergency and foam quality 20.00
PERSOFT® EF Sodium Laureth Sulfate, Water Improves detergency and foam quality 10.00
DIAPON® K-SF Sodium Methyl Cocoyl Taurate, Water Improves detergency and foam quality 10.00
SOFTILT® AS-L Sodium Lauroyl Methylaminopropionate, Water Improves detergency; thickener 10.00
NONION DL-40HN(W) PEG-75 Dilaurate, Water Thickener; improves foam volume 2.00
MACBIOBRIDE® MG-T PEG-120 Methylglucose Triisostearate, Water Thickener 0.60
UNISAFE® PGML Propylene Glycol Laurate Thickener 0.50
Preservative Preservative q.s.
C Citric Acid pH adjuster q.s.
D NONION OT-80 Polysorbate 80 Solubilizer 0.80
Fragrance q.s.

Typical Physical Properties: pH (undiluted solution) 6.0; viscosity (undiluted solution, 25 °C) 3,000–5,000 mPa·s.

Preparation Method

  1. Measure the phase-A ingredients and stir at room temperature until evenly mixed.
  2. Heat the phase-A ingredients to 80±5 ℃ and add the phase-B ingredients.
  3. Add the phase-C ingredient and stir at 80±5 ℃ until evenly mixed.
  4. After cool down to 25±5 ℃, add the phase-D ingredients before mixed at 25±5 ℃, and stir until evenly mixed.

This formula is result by our best efforts. But, this formula does not guarantee performance, safety, stability, or commercial property rights for your products.

Rich Foam Non-silicon Shampoo

Formulation Table

Phase Ingredient INCI Purpose %
A Water Balance
Polyquaternium-10 Conditioning; thickener 0.50
B ANON BDF-R Cocamidopropyl Betaine, Water Improves detergency and foam quality 16.70
PERSOFT® EF Sodium Laureth Sulfate, Water Improves detergency and foam quality 16.40
LUMINOVEIL® HS-L Sodium Lauroyl Hydroxyethyl Beta-Alaninate, Water Improves detergency and foam elasticity 3.00
RG・CO・P Glycerin Moisturizer 2.00
STAFOAM® DL Lauramide DEA Thickener; improves foam volume 1.50
Lipidure®-C Polyquaternium-64, Water, Phenoxyethanol Conditioning 0.10
Glycosyl Trehalose Moisturizer 0.10
Preservative Preservative q.s.
C Citric Acid pH adjuster q.s.
D NONION OT-80 Polysorbate 80 Solubilizer 0.80
Fragrance q.s.

Typical Physical Properties:pH (undiluted solution) 6.0; viscosity (undiluted solution, 25 °C) 870 mPa·s

Preparation Method

  1. Measure the phase-A ingredients and stir at room temperature until evenly mixed.
  2. Heat the phase-A ingredients to 80±5 ℃ and add the phase-B ingredients.
  3. Add the phase-C ingredient and stir at 80±5 ℃ until evenly mixed.
  4. After cool down to 25±5 ℃, add the phase-D ingredients before mixed at 25±5 ℃, and stir until evenly mixed.

This formula is result by our best efforts. But, this formula does not guarantee performance, safety, stability, or commercial property rights for your products.

High-blending Oil Shampoo

Formulation Table

Phase Ingredient INCI Purpose %
A Water Balance
Polyquaternium-10 Conditioning; thickener 0.25
B LUMINOVEIL® HS-L Sodium Lauroyl Hydroxyethyl Beta-Alaninate, Water Improves detergency, foam quality, and foam elasticity 50.00
DIAPON® HF-SF Sodium Caproyl Methyltaurate, Water Improves foam volume 15.00
ANON BDF-SF Cocamidopropyl Betaine, Water Improves detergency and foam quality 11.00
Preservative Preservative q.s.
C UNIOX® ST-40E Sorbeth-40 Tetraoleate Solubilizer 6.00
Olea Europaea (Olive) Fruit Oil Conditioning 2.00
Argania Spinosa Kernel Oil Conditioning 1.00
D Citric Acid pH adjuster q.s.
E NONION OT-80 Polysorbate 80 Solubilizer 0.80
Fragrance q.s.

Typical Physical Properties:pH (undiluted solution) 6.1; viscosity (undiluted solution, 25 °C) 330 mPa·s

Preparation Method

  1. Measure the phase-A ingredients and stir at room temperature until evenly mixed.
  2. Heat the phase-A ingredients to 80±5 ℃ and add the phase-B ingredients.
  3. Separately, measure the phase-C ingredients and stir at 80±5 ℃ until evenly mixed.
  4. Add (3) solution to (2) solution and stir until evenly mixed.
  5. Add the phase-D ingredient and stir at 80±5 ℃ until evenly mixed.
  6. After cool down to 25±5 ℃, add the phase-E ingredients before mixed at 25±5 ℃, and stir until evenly mixed.

This formula is result by our best efforts. But, this formula does not guarantee performance, safety, stability, or commercial property rights for your products.

Moist Shampoo

Formulation Table

Phase Ingredient INCI Purpose %
A Water Balance
Polyquaternium-10 Conditioning; thickener 1.20
B DIAPON® K-SG Sodium Taurine Cocoyl Methyltaurate, Water Improves detergency and foam quality; moisturizer 18.60
ANON BDF-SF Cocamidopropyl Betaine, Water Improves detergency and foam quality 15.00
SOFTILT® AS-L Sodium Lauroyl Methylaminopropionate, Water Improves detergency; thickener 11.00
Dipropylene Glycol Moisturizer 4.00
Butylene Glycol Moisturizer 2.00
Caprylyl/Capryl Glucoside Improves foam volume 2.00
Disodium Cocoyl Glutamate Improves foam volume 1.50
STAFOAM® DL Lauramide DEA Thickener; improves foam volume 0.90
Preservative Preservative q.s.
C Citric Acid pH adjuster q.s.
D NONION OT-80 Polysorbate 80 Solubilizer 0.80
Fragrance q.s.

Typical Physical Properties:pH (undiluted solution) 5.9; viscosity (undiluted solution, 25 °C) 1,450 mPa·s

Preparation Method

  1. Measure the phase-A ingredients and stir at room temperature until evenly mixed.
  2. Heat the phase-A ingredients to 80±5 ℃ and add the phase-B ingredients.
  3. Add the phase-C ingredient and stir at 80±5 ℃ until evenly mixed.
  4. After cool down to 25±5 ℃, add the phase-D ingredients before mixed at 25±5 ℃, and stir until evenly mixed.

This formula is result by our best efforts. But, this formula does not guarantee performance, safety, stability, or commercial property rights for your products.

Smooth and Volume-rich Shampoo

Formulation Table

Phase Ingredient INCI Purpose %
A Water Balance
Polyquaternium-10, Polyquaternium-7 Conditioning; thickener 0.90
B DIAPON® K-SF Sodium Methyl Cocoyl Taurate, Water Improves detergency and foam quality 30.00
ANON BL-SF Lauryl Betaine, Water Improves detergency and foam quality 15.00
SOFTILT® AX-L Sodium Taurine Lauroyl Methyl Beta-Alaninate, Water Improves detergency; thickener 4.80
ANON LA Disodium Lauriminodiacetate, Water Improves detergency and foam quality 4.20
NONION DL-40HN(W) PEG-75 Dilaurate, Water Thickener; improves foam volume 2.00
Dipropylene Glycol Moisturizer 2.00
STAFOAM® MF Cocamide MEA Thickener; improves foam volume 0.80
Disodium Cocoyl Glutamate Improves foam volume 0.50
Preservative Preservative q.s.
C Citric Acid pH adjuster q.s.
D NONION OT-80 Polysorbate 80 Solubilizer 0.80
Fragrance q.s.

Typical Physical Properties:pH (undiluted solution) 5.7; viscosity (undiluted solution, 25 °C) 370 mPa·s

Preparation Method

  1. Measure the phase-A ingredients and stir at room temperature until evenly mixed.
  2. Heat the phase-A ingredients to 80±5 ℃ and add the phase-B ingredients.
  3. Add the phase-C ingredient and stir at 80±5 ℃ until evenly mixed.
  4. After cool down to 25±5 ℃, add the phase-D ingredients before mixed at 25±5 ℃, and stir until evenly mixed.

This formula is result by our best efforts. But, this formula does not guarantee performance, safety, stability, or commercial property rights for your products.